MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lushan L-5R Polyethylene Copolymer Adhesive for Steel Pipe Coating
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and proved with excellent performance in the widely applications of pipeline projects both in China and international market. The purpose of the adhesive is to bond the epoxy layer to the top coat. Copolymer adhesive resin Lushan L-5R series in mainly used as adhesive layer in 3 layers polyethylene system (3LPE) for steel pipe against corrosion coating system in oil and gas pipeline and high pressure water pipeline. Copolymer adhesive resin Lushan L-5R series has good properties such as high bonding strength, long-term stability, wide compatibility, easy processing, etc. Copolymer adhesive resin Lushan L-5R series designed to meet with requirements of the following National and international standards, under the condition that appropriate industrial processing method are applied under a continuous quality control system and when used in combination copolymer adhesive resin Lushan L-5R& polyethylene compound top coats EJ-1 and compatible powder epoxy.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Melt Index of Compound 2.3 g/10 min2.3 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psiASTM D638
Elongation at Break 860 %860 %ASTM D638
Peel Strength >= 90.0 kN/m>= 514 pli60+5°C; ISO 21809-1
 >= 130 kN/m>= 742 pli50+5°C; ISO 21809-1
 >= 160 kN/m>= 913 pli20+5°C; ISO 21809-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °FASTM D2117
Maximum Service Temperature, Air 60.0 °C140 °F
Vicat Softening Point 104 °C219 °FASTM D1525
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Brittleness Temperature -70.0 °C-94.0 °FASTM D746
 
Descriptive Properties
Appearancegranule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lushan EJ-1 Polyethylene compounds for steel pipe top coats

PLUSH001 / 149999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.