MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Envalior ForTii® Ace WX53-FC PPA-GF50 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® Ace WX53-FC has best in class high temperature and wet mechanical performance, weldline strength and weldline strength retention in hot water and steam. Features: USP class VI classified, Drinking Water Grade. 50% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 g/ccDry; ISO 1183
Moisture Absorption 1.50 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 71.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 83.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 100 MPa
@Temperature 160 °C
ISO 527-1/-2
 110 MPa
@Temperature 150 °C
ISO 527-1/-2
 180 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 210 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 230 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 260 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 270 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 280 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 340 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
Elongation at Break 2.1 %
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 2.2 %
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 2.2 %
@Temperature 100 °C
Dry; ISO 527-1/-2
 2.3 %
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 2.3 %
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 2.3 %
@Temperature 120 °C
Dry; ISO 527-1/-2
 2.5 %
@Temperature -40.0 °C
Dry; ISO 527-1/-2
 4.2 %
@Temperature 150 °C
ISO 527-1/-2
 4.3 %
@Temperature 160 °C
ISO 527-1/-2
 4.4 %
@Temperature 200 °C
ISO 527-1/-2
 4.6 %
@Temperature 180 °C
ISO 527-1/-2
Tensile Modulus 6300 MPa
@Temperature 200 °C
ISO 527-1/-2
 6800 MPa
@Temperature 180 °C
ISO 527-1/-2
 7600 MPa
@Temperature 160 °C
ISO 527-1/-2
 8500 MPa
@Temperature 150 °C
ISO 527-1/-2
 16000 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 17000 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 17200 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 17500 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 18000 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 18500 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 19000 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
Flexural Strength 380 MPaCond; ISO 178
 420 MPaDry; ISO 178
Flexural Modulus 6600 MPa
@Temperature 200 °C
ISO 178
 7100 MPa
@Temperature 180 °C
ISO 178
 8300 MPa
@Temperature 160 °C
ISO 178
 16700 MPa
@Temperature 120 °C
ISO 178
 17500 MPa
@Temperature 23.0 °C
Dry; ISO 178
 18000 MPa
@Temperature 23.0 °C
Cond; ISO 178
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 13.5 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eA
 14.5 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 15.5 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 43.0 kV/mmDry; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 333 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 305 °CDry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7926 / 291362

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.