MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient PolyAdd™ 1909-T Antiblock PEC Antiblock Additive Concentrate, Talc Filled  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes:

1909-T is a heavily loaded concentrate for use where freedom from blocking is important. The talc used in this concentrate has been specifically developed by the producer as an antiblock additive. Its performance should be very similar to the performance of equal loadings of diatomaceous earth.

Description/Features:

  • Talc Filled

Market:

  • Film

Processing Method:

  • Blown Film
  • Cast Film

Note: Because of the high surface area of the antiblock additive, and with certain minor resin additives, this concentrate can discolor after long storage times. Caution is advised to use 1909-T on a first in, first out basis to prevent discoloration. Acceptable for FDA applications depending on end use.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
High Load Melt Index 4.6 - 7.3 g/10 min
@Load 21.6 kg,
Temperature 190 °C
4.6 - 7.3 g/10 min
@Load 47.6 lb,
Temperature 374 °F
Procedure A - Manual Operation
 
Descriptive Properties
Antiblock AdditiveTalc
Base ResinLDPE
Loading50 %
Product FormUnderwater Cut Pellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PO3044 / 44862

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.