MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Features:
  • Good abrasion resistance
  • Pleasing surface appearance
  • Good chemical resistance
  • High impact resistanceHigh rigidity
  • Low shrinkage
  • Solvent resistance
  • High strength
  • Good thermal stability
  • Good toughness
  • Low warpage
  • Injection molding

Form: Pellets

Information provided by Chase Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/in0.125 in; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 43.4 MPa6300 psiASTM D638
Elongation at Break 230 %230 %ASTM D638
Flexural Strength 56.9 MPa8250 psiASTM D790
Flexural Modulus 1.45 GPa210 ksiASTM D790
Izod Impact, Notched 10.1 J/cm19.0 ft-lb/in0.125 in; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FUnannealed; ASTM D648
Vicat Softening Point 199 °C390 °FRate A; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Techmer ES Plastiblend® ABS/PA 1700
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced
Americhem Engineered Compounds ColorFast® NYA1000 Nylon/ABS Alloy

PCHA008 / 28004

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.