MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking resistance, UV stabilized.

Applications: rotational molded items with good stiffness, septic tanks, ordinary containers.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.938 g/ccASTM 1505-68
Environmental Stress Crack Resistance 400 hourASTM D1693
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238-7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 15.0 MPaASTM D638-72
Elongation at Break >= 900 %ASTM D638
Flexural Modulus 650 MPaASTM D790
Charpy Impact, Notched 18.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.480 W/m-KASTM D177
Vicat Softening Point 115 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 131 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
Ethydco Advancene™ EM-3405-UVH MDPE Roto Molding Resin

PIPC245 / 149707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.