MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sodium Iodide, NaI
Categories: Ceramic; Halide

Material Notes: White cubic crystals, hygroscopic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.67 g/cc
Molecular Weight 149.894 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.0000570cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 157.4 J/g
CTE, linear 47.5 µm/m-°C
Specific Heat Capacity 0.3476 J/g-°CCrystal
Melting Point 660 °C
Boiling Point 1304 °C
Heat of Formation -287.8 kJ/molCrystal
 
Descriptive Properties
CAS Number7681-82-5
ColorWhite
Crystal StructureCubic
SolubilityVery Soluble in H2O; Soluble in EtOH and Acetone

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal
Mateck Window Grade Zinc Selenide, ZnSe
Sodium Bromide, NaBr
Zinc Selenide, ZnSe
Lead (II) Sulfide, PbS

EINOR0764 / 3896

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.