MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Refractory Composites AL-HARD AL-HARD RIGIDIZER HARDENER
Categories: Ceramic

Material Notes: ZRCI AL-HARD Rigidizer/Hardener is used to increase the hardness of ZRCI Refractory Sheet products. AL-HARD is comprised of Aluminum Oxide and Phosphoric Acid in a water base. Refractory Sheet products treated with AL-HARD are ready for use after drying. When a chemical bond forms it hardens the fibrous material. The degree of hardening depends on the amount of AL-HARD used. AL-HARD is non-flammable and is not affected by freezing. It can be applied by immersing, spraying, brushing or sponging on many of ZRCI`s Refractory Sheet products.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 20 %20 %
pH 1.31.3
 
Component Elements PropertiesMetricEnglishComments
Al2O3 16 - 20 %16 - 20 %
Free Water 68 - 75 %68 - 75 %
 
Descriptive Properties
ColorOpaque White
H3PO4, %9 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-201 Refractory Sheet
Zircar Refractory Composites RS-99W Refractory Sheet
Zircar Refractory Composites RSLE-57 Refractory Sheet
AR-Glass Fiber, Generic
Zircar Refractory Composites RS-200 Refractory Sheet

CZRCI00 / 2863

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.