MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite SUMILITE® ALC-1331 CCL Material
Categories: Polymer

Material Notes: Aluminum Base CCL High heat releasing material for LED lighting , power module etc based on aluminum base polymer. It is supplied as sheet for printed wiring boards.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.30 %0.30 %D-24/23
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 1.40 kN/m7.99 pliE-1000/125; 35umCF
 1.50 kN/m8.56 pliA; 35umCF
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.60e+13 ohm-cm6.60e+13 ohm-cmC-96/40/90
 3.50e+15 ohm-cm3.50e+15 ohm-cmA
Surface Resistance 1.20e+14 ohm1.20e+14 ohmC-96/40/90
 2.10e+15 ohm2.10e+15 ohmA
Dielectric Constant  7.2
@Frequency 1e+6 Hz
7.2
@Frequency 1e+6 Hz
C-96/20/65
 7.7
@Frequency 1e+6 Hz
7.7
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Dissipation Factor  0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
C-96/20/65
 0.025
@Frequency 1e+6 Hz
0.025
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Comparative Tracking Index 600 V600 VA; IEC; Tracking Resistance
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.50 W/m-K17.4 BTU-in/hr-ft²-°FA; Hot Wire
 3.00 W/m-K20.8 BTU-in/hr-ft²-°FA; Laser Flash
Glass Transition Temp, Tg 96.0 °C205 °F5°C/min
 100 °C212 °F20°C/min
 100 °C212 °F10°C/min
Flammability, UL94 V-0V-0Flame Resistance
 
Descriptive Properties
Breakdown Voltage AC5A; 25mmf pattern
 5E-1000/125; 25mmf pattern
Breakdown Voltage DC>10A; 25mmf pattern
 >10E-1000/125; 25mmf pattern

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 RF Paper Phenolic
Sumitomo Bakelite SUMILITE® ELC-4972R&S Glass Epoxy Laminate

PSUMIT119 / 193924

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.