MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Inov Chem PE-2315 Casting Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Introduction: This series is mainly used for producing polyurethane elastomer and the molecular weight can be adjusted according to customer request.

Applications: This series of polyester polyol is mainly used for producing casting polyurethane especially middle and high hardness prepolymer. The pre-polymer is mainly used for producing polyurethane sieve plate, caster, roller, pad, rod and molded potting product.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 300 - 600 cP
@Temperature 75.0 °C
300 - 600 cP
@Temperature 167 °F
Molecular Weight 1500 g/mol1500 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.50<= 0.50[mgKOH/g]
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.030 %<= 0.030 %
 
Descriptive Properties
Color=30APHA
OH value73-79 mgKOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM344 / 312873

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.