MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel 154 CM Martensitic Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than 440C. For knife makers, it offers better edge retention than 440C. It also has higher attainable hardness and better through hardening characteristics than 440C.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 58.5
Modulus of Elasticity 207 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.02 µm/m-°C
@Temperature -73.3 - 21.1 °C
 10.35 µm/m-°C
@Temperature 21.0 - 149 °C
 10.91 µm/m-°C
@Temperature 21.0 - 260 °C
 11.86 µm/m-°C
@Temperature 21.0 - 482 °C
Thermal Conductivity 24.2 W/m-K
@Temperature 95.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.05 %
Chromium, Cr 14 %
Iron, Fe 80.95 %As Remainder
Molybdenum, Mo 4.0 %
 
Descriptive Properties
Total Carbide Volume; %17.5
Wear Resistance; mg49Pin abrasion method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Martensitic
Overview of materials for Stainless Steel
Crucible Steel CPM® 154 Tool Steel
6082-O Aluminum
403 Stainless Steel, annealed, sheet

NCRUC027 / 16020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.