MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Bynel® 50E561 Anhydride-Modified Polypropylene Adhesive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E561 and 50E571 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylene (PP) resins.

Applications: Bynel® Series 5000 resins adhere to a variety of materials. They are most often used to adhere to PP, EVOH, and polyamide. These resins are designed for applications in which EVOH or polyamide is melt coextruded with PP or PP copolymers. Bynel® 50E561 and 50E571 can be used in coextrusion processes including blown film, melt and solid phase thermoforming, and cast film or sheet. Bynel® 50E571 can also be used in extrusion blow molding. Bynel® 50E561 and 50E571 provide outstanding adhesion to EVOH.

Physical properties of Bynel® Series 5000 resins are typical of polypropylene resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Viscosity 1.20e+6 cP
@Shear Rate 50 1/s,
Temperature 210 °C
1.20e+6 cP
@Shear Rate 50 1/s,
Temperature 410 °F
estimated from log-log graph.
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.0 °C203 °FFreezing point via DSC/ASTM D3418
 141 °C286 °FMelting point via DSC/ASTM D3418
Vicat Softening Point 109 °C228 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 °C455 °FExtruder forward zone and adapter for film or coating with EVA or EVOH
Nozzle Temperature 235 °C455 °FDie

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Fusabond® MZ203D Polypropylene Impact Copolymer
Dow Bynel® 50E571 Anhydride-Modified Polypropylene Adhesive Resin
Overview of materials for Polypropylene, Extrusion Grade
Bamberger Polymers Bapolene® 5010NB Polypropylene, Extrusion Grade
DuPont Fusabond® MD511D Polypropylene Homopolymer

PDUPC6 / 33587

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.