MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond HL138 Anaerobic Retaining Compound
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which eliminates wear, erosion, and pitting. Permabond HL138 cures to a tough cross-linked plastic and provides excellent environmental and temperature resistance. Since Permabond® HL138 can fill up the inner space, shaft-hub assemblies can be made with a clearance fit and eliminates an expensive press fit, while actually increasing the push out force. Permabond® HL138 develops full strength in a few hours on a large variety of substrates and is used on high speed production lines.

Features & Benefits:

  • Simple one-part fast cure low viscosity system
  • Excellent shear strength
  • Good environmental resistance

Information provided by Permabond.

Key Words: MIL-R-46082B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Viscosity 150 - 300 cP
@Temperature 25.0 °C
150 - 300 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 16.0 MPa2320 psisteel collar and pin shear; ISO 10123
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 11.0 kV/mm279 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  4.98 min
@Temperature 23.0 °C
0.0830 hour
@Temperature 73.4 °F
Zinc, handling strength
 10.2 min
@Temperature 23.0 °C
0.170 hour
@Temperature 73.4 °F
M10 steel, handling strength
 15.0 min
@Temperature 23.0 °C
0.250 hour
@Temperature 73.4 °F
Zinc, working strength
 15.0 min
@Temperature 23.0 °C
0.250 hour
@Temperature 73.4 °F
Aluminum, handling strength
 180 min
@Temperature 23.0 °C
3.00 hour
@Temperature 73.4 °F
M10 steel, working strength
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
M10 steel, full strength
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Aluminum, working strength
 
Descriptive Properties
AppearanceGreenUncured
Maximum Gap Fill (mm)0.127
Maximum Thread SizeM20
Strength Retention50% at 150°CRelative to 0°C
 80% at 100°CRelative to 0°C
 93% at 50°CRelative to 0°C
Torque Strength (N m)20M10 steel, break
 36M10 steel, prevail
UV FluorescenceNoUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERMA22 / 56130

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.