MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vicone High Performance Rubber VicoFluor™ 06FK-BR High Performance Fluoroelastomer Rubber
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Meets ASTM D2000 fluoroelastomer 60 Durometer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.11 g/cc0.0762 lb/in³ASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5959ASTM D2240
Tensile Strength 12.2 MPa1770 psiASTM D412
Elongation at Break 303 %303 %ASTM D412
Compressive Modulus  0.00550 GPa
@Strain 5.0 %
0.798 ksi
@Strain 5.0 %
ISO-7743
 0.00640 GPa
@Strain 10 %
0.928 ksi
@Strain 10 %
ISO-7743
 0.00730 GPa
@Strain 20 %
1.06 ksi
@Strain 20 %
ISO-7743
 0.00780 GPa
@Strain 25 %
1.13 ksi
@Strain 25 %
ISO-7743
Compression Set 22 %
@Temperature 200 °C,
Time 79200 sec
22 %
@Temperature 392 °F,
Time 22.0 hour
ASTM D395
 
Descriptive Properties
ColorBrown
Effect of Liquids - Change in Elongation (%)-22ASTM D471
Effect of Liquids - Change in Hardness (%)-3ASTM D471
Effect of Liquids - Change in Tensile Strength (%)-26ASTM D471; 23°C; 70 h
Effect of Liquids - Change in Volume after Oil Immersion (%)4.5ASTM D471
Heat Aging - Change in Elongation (%)-8ASTM D573; 275°C; 70h
Heat Aging - Change in Hardness (%)5ASTM D573; 275°C; 70h
Heat Aging - Change in Tensile Strength (%)-11ASTM D573; 275°C; 70h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Applied Composites 120 Polyester SMC
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE
E-Glass Fiber, Generic
Overview of materials for PVC, Foam Grade

PAVICON995 / 108915

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.