MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Struktol V-PEAS LA LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: STRUKTOL® V-PEAS LA is a very effective lubricant with externally lubricating properties which has no negative impact on clarity in extrusion, calendering, or injection molding. STRUKTOL® V-PEAS LA is noted to have ideal characteristics for calendared sheet where clarity is critical and where lower cost in performance is needed to replace montanic esters.

Applications: STRUKTOL® V-PEAS LA is a very compatible complex ester lubricant with lower acid value than STRUKTOL® V-PEAS, and is especially suited for calendared PVC sheet. It also has application in extrusion, blow molding, and injection molding formulations.

Information provided by Struktol

Sanctioned for use by the Food and Drug Administration in a number of applications, listed in the following sections of Title 21 of the Code of Federal Regulations: 178.3690

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.017 g/cc1.017 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Value 5.0 - 125.0 - 12
 
Thermal PropertiesMetricEnglishComments
Dropping Point 52.0 - 60.0 °C126 - 140 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
AppearanceOff-white prill or pastille

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTRUK45 / 69272

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.