MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant Polylactic Acid Natural Color 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Clariant’s PLA 3D printer filament uses NatureWorks Ingeo™ Biopolymer 3D850 PLA for its excellent material performance and printability and is further optimized with Clariant Hostanox® P-EPQ® and Hostavin® ARO 8 to improve the heat stability and resistance to thermo-oxidative degradation and yellowing.

General properties:

  • Biodegradable and derived from renewable resources
  • Semi-crystalline thermoplastic polyester
  • High tensile strength
  • Safe to print
Optimized benefits:
  • Reduced thermo-oxidative degradation
  • Minimized undesired yellowing due to ultraviolet light
Applications:
  • Models
  • Education
  • Prototypes

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.255 g/ccISO 1183
pH 5.71% in H2O
Melt Flow 7.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 73.0 MPaInjection molded, 50 mm/min; ISO 527
Elongation at Break 5.0 %Injection molded, 50 mm/min; ISO 527
Modulus of Elasticity 3.37 GPaInjection molded, 1 mm/min; ISO 527
Flexural Strength 65.0 MPaInjection molded; ISO 178
Flexural Modulus 2730 MPaInjection molded; ISO 178
Charpy Impact, Notched 0.303 J/cm²Injection molded; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CDSC; ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C3D printed XY / flat at 210°C; ISO 75
 80.0 - 90.0 °CInjection molded; ISO 75
Glass Transition Temp, Tg 61.0 - 62.0 °CDSC; ISO 11357
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 220 °CPrint Temperature
 
Descriptive Properties
Bed Adhesiondirectly on glass, polyimide film or a PEI surface; a thin coating of EVA or PVP glue may applied to the bed to enhance adhesion
Bed Temperatureideally heated up to 70°C
Fan Settingsmedium to high
Heat stabilityHeat deflection temperature of the 3D printed part(s) may be increased by annealing at 80-130°C
Print Speed30-70 mm/s
Volume4.95 cm3ISO 1183

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Polylactic Acid White 3D Printer Filament
Essentium High Performance PLA Additive Manufacturing Filament
Clariant Polylactic Acid Black 3D Printer Filament
Overview of materials for Polylactic Acid (PLA) Biopolymer
Clariant Polylactic Acid Red 3D Printer Filament

PCLAR00031 / 232108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.