Water-clear, semi-rigid polyurethane formulated Key Properties: - Excellent physical properties after RT cure
- Free of mercury, MOCA or TDI
- Excellent optical clarity as well as U.V. stability
- Specially formulated for mass castings into either tin or platinum silicone molds
Applications: - For room temperature hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F + 16 hours at 150°F Cure 2: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |