MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: High melt strength for thick sheet extrusion.

Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile Extrusion

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
ASTM D2240
Tensile Strength 51.7 MPaASTM D412
Elongation at Break 600 %ASTM D412
100% Modulus 0.00550 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00970 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 4020 psiASTM D790
Tear Strength 140 pliTrouser; ASTM D470
Graves Tear Strength 450 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 63H18, 1000g; ASTM D3389 B
Tensile Set 10 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CDSC
Glass Transition Temp, Tg -44.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Zone 1 183 °CExtrusion
Zone 2 188 °CExtrusion
Zone 3 194 °CExtrusion
Zone 4 199 °CExtrusion
Adapter Temperature 199 °CExtrusion
Die Temperature 199 °CZone 1, Extrusion
 199 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission

PNOVEON050 / 55317

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.