MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.928 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45ASTM D2240
Tensile Strength at Break 9.10 MPa510 mm/min; ASTM D412A
Tensile Stress at Strain 1.72 MPa
@Strain 100 %
510 mm/min; ASTM D412A
 3.14 MPa
@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 1000 %510 mm/min; ASTM D412A
Tear Strength 29.8 kN/mDie C, 510 mm/min; ASTM D624
Compression Set 16 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact, Unspecified Rating
 
Descriptive Properties
FeaturesFood Contact Acceptable
 General Purpose
FormsPellets
Generic NameStyrene Butadiene Block Copolymer (SBC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Interior Parts
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Sofprene T® 5405.A50 SBS TPE
Avient Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC)
Kraton® D2109 DS-N (SBS) Compound
Kraton® D2109 DS-W (SBS) Compound
I. Stern Q Resin Clear Styrene Butadiene Copolymer

PH1PN8097 / 101933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.