MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 (a) when used unmodified and according to good manufacturing practices for food contact applications, including packing or holding food during cooking. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/cc
Thickness 25.0 microns
Melt Flow 2.3 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 7.6.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 13.1 MPaMolded property
Film Tensile Strength at Yield, MD 7.60 MPa
Film Tensile Strength at Yield, TD 7.60 MPa
Tensile Strength, Yield 10.3 MPaMolded property
Film Elongation at Break, MD 510 %
Film Elongation at Break, TD 760 %
Elongation at Break 900 %Molded value
Elmendorf Tear Strength MD 325 g
Elmendorf Tear Strength TD 520 g
Elmendorf Tear Strength, MD 13.0 g/micron
Elmendorf Tear Strength, TD 20.8 g/micron
Dart Drop 12.8 g/micron
Film Tensile Strength at Break, MD 62.7 MPa
Film Tensile Strength at Break, TD 39.3 MPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 99.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 0.90 %
Gloss 95 %45°
 
Processing PropertiesOriginal ValueComments
Processing Temperature 274 °CFilm extrusion temperature
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2047G Linear Low Density Polyethylene
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade

PDW435 / 34504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.