MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik VESTANAT® T 1890 E Polyisocyanate
Categories: Polymer

Material Notes: VESTANAT T 1890 is a cycloaliphatic polyisocyanate based on isophorone diisocyanate. It contains isocyanurate groups and has a NCO-functionality between 3 and 4. It is used as a crosslinker in paints based on suitable polyesters, acrylates, flexible medium-oil or short-oil alkyd resins and other resins containing OH-groups.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc
@Temperature 15.0 °C
0.0383 lb/in³
@Temperature 59.0 °F
DIN 51 757
Solids Content 69 - 71 %69 - 71 %DIN EN ISO 3251
Viscosity 0.65 - 1.15 cP
@Temperature 23.0 °C
0.65 - 1.15 cP
@Temperature 73.4 °F
DIN EN ISO 3219
 
Thermal PropertiesMetricEnglishComments
Flash Point 30.0 °C86.0 °Fclosed cup; DIN EN ISO 1523
 
Descriptive Properties
Hazen Color Index, max150DIN ISO 6271
NCO content (% wt)11.7-12.3DIN EN ISO 11 909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTANAT® T 1890 L Polyisocyanate
Overview of materials for Phenolic; Unreinforced; Molded
Graphite, Carbon, C
Evonik VESTANAT® IPDI Polyisocyanate
Evonik HEMA 97 Hydroxyester

PHUMB404 / 81406

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.