MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Brazilian Rosewood Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Mechanical properties reported according to ASTM D143 at 12 wt% moisture content.

Key Words: Dalbergia nigra, timber, lumber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.800 g/cc0.800 g/ccGreen
Density 0.850 g/cc0.0307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 10900 N2450 lb (f)Side Hardness, Green
 12100 N2720 lb (f)Side Hardness, 12% Moisture
Modulus of Rupture 0.0972 GPa14.1 ksiStatic Bending, Green
 0.131 GPa19.0 ksiStatic Bending, 12% Moisture
Flexural Modulus 12.7 GPa1840 ksiStatic Bending, Green
 13.0 GPa1890 ksiStatic Bending, 12% Moisture
Compressive Strength 38.0 MPa5510 psiParallel to Grain, Green
 66.2 MPa9600 psiParallel to Grain, 12% Moisture
Shear Strength 14.5 MPa2100 psiParallel to Grain, 12% Moisture
 16.3 MPa2360 psiParallel to Grain, Green
Work to Maximum Load 0.0910 J/cm³13.2 in-lb/in³Static Bending, Green
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.9 %2.9 %radial; from green to oven-dry condition based on initial condition when green
 2.9 %2.9 %Radial Shrinkage Green to Oven Dry
 4.6 %4.6 %Tangential Shrinkage Green to Oven Dry
 4.6 %4.6 %tangent
 8.5 %8.5 %volume
 8.5 %8.5 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
CategoryHardwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
White Oak
Balsam Poplar Cottonwood Wood
Berlinia Wood
Bigleaf Hickory Wood
Bigleaf Maple Wood

PTSU063 / 100547

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.