MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch™ 2228 Rubber Mastic Tape
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-stable mastic adhesive. The tape is made 65 mils (1.65 mm) thick for quick application build-up. It is designed for electrical insulating and moisture sealing applications. Scotch 2228 can be used on copper or aluminum conductors rated at 90°C, with an emergency overload rating of 130°C. It offers excellent resistance to moisture and ultraviolet exposure and is intended fro both indoor and weather exposed outdoor applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.15 %0.15 %ASTM D570
Water Vapor Transmission 1.55 g/m²/day0.0998 g/100 in²/dayASTM D3833
Thickness 1650 microns65.0 milASTM D4325
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.03 MPa149 psiASTM D4325
Elongation at Break 1000 %1000 %ASTM D4325
Peel Strength 0.110 kN/m0.625 pliAdhesion to Polyethylene; ASTM D1000
 0.1643 kN/m0.9375 pliAdhesion to Steel; ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.53.5ASTM D4325
Dielectric Strength 19.7 kV/mm500 kV/inDry; ASTM D4325
 19.7 kV/mm500 kV/inWet; ASTM D4325
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35182 / 169929

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.