MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Silberline Aquasil® "BP" SN
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and system compatibility with a broad range of coating vehicles. This range of aluminum pigment grades offers aesthetics to meet virtually any formulating requirement.

Applications: General Industrial; Waterborne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/cc
Bulk Factor 0.0800.080
Volatiles 37 %37 %
Particle Size 14 µm14 µm
Particle Mesh Size <= 325 Mesh<= 325 Mesh1% retained
 
Descriptive Properties
Aluminum Flake, wt%54
CategoryNon-leafing
SolventsMineral Spirits/High Aromatic/Nitroethane/Propylene Glycol Ether

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2218-T61 (Includes Creep/Rupture/Fatigue Data)
Silicon Nitride, HIP-SN
Cast Stainless Steel CA6NM, ASTM A743
AISI 4140 Steel, oil quenched, 50 mm (2 in.) round (845°C (1550°F) quench, 595°C (1100°F) temper)
Tin, Sn (Gray)

ESIBER088 / 5843

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.