MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 12C27M Strip Steel
Categories: Metal; Ferrous Metal; Martensitic; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik 12C27M is a martensitic stainless chromium steel developed for the manufacture of kitchen tools with high demands on wear- and corrosion resistance properties.

After heat treatment the steel grade is characterized by:

  • High hardness which gives good wear resistance.
  • Good corrosion resistance
  • Sandvik 12C27M is mainly used for kitchen tools, such as different types of knives and scissors, that need to tolerate dish-washing.

    Information provided by Sandvik

    ASTM 420, 440A; EN 1.4034, 1.4037

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.80 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell B <= 94Soft annealed
     91.4 - 103.4annealed
     94 - 107cold rolled
    Hardness, Rockwell C 52.5tempering temperature- 350°C
     57.8tempering temperature- 150°C
    Hardness, Vickers <= 215soft annealed
     200 - 270annealed
     215 - 315cold rolled
    Tensile Strength <= 700 MPasoft annealed
     650 - 850 MPaannealed
     700 - 1000 MPacold rolled
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C 0.52 %
    Chromium, Cr 14.5 %
    Iron, Fe 84 %As Balance
    Manganese, Mn 0.60 %
    Phosphorus, P <= 0.025 %
    Silicon, Si 0.40 %
    Sulfur, S <= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Sandvik 12C27 Strip Steel
    AISI 440 Stainless Steel
    Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
    440A Martensitic Stainless Steel (UNS S44002)
    Outokumpu 4021 Martensitic Stainless Steel

    NSANDV277 / 19171

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.