MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sibur 1030-13 Compound OMN Polyvinyl Chloride (PVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a period of 20 minutes. For insulation of wires and cables operating in intervals of temperatures from -40°C to 70°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.55 g/cc0.0524 - 0.0560 lb/in³
Water Absorption <= 0.40 %<= 0.40 %
Collected Volatile Condensable Material <= 2.5 %<= 2.5 %Loss in mass at 160°C during 6 hours
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 15.0 MPa>= 2180 psi
Elongation at Break >= 200 %>= 200 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 5.00e+10 ohm-cm
@Temperature 70.0 °C
>= 5.00e+10 ohm-cm
@Temperature 158 °F
 >= 1.00e+13 ohm-cm
@Temperature 20.0 °C
>= 1.00e+13 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -30.0 °C<= -22.0 °F
Decomposition Temperature >= 200 °C>= 392 °FThermal stability, for 80 minutes
Flammability Test <= 15<= 15In seconds, method A
 
Descriptive Properties
ColorNon-colored, black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIB051 / 67614

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.