MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 El Mar® Mid Ash Heavy Duty GEO, SAE Grade 40
Categories: Fluid; Lubricant

Material Notes: Phillips 66® El Mar Mid Ash Heavy Duty GEO is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natural gas engines. It is particularly recommended for use in natural gas engines and dual-fuel engines burning sour gas or landfill gas. El Mar Mid Ash Heavy Duty GEO is formulated with field-proven performance additives to provide excellent resistance to oxidation and nitration, protect against piston scuffing and wear, and minimize the formation of sludge and piston deposits for good engine cleanliness. It has a high alkaline reserve (TBN) to protect engines operating under corrosive conditions, such as when burning sour gas, digester gas or landfill gas.

Applications:

  • 4-stroke cycle gas and dual-fuel engines burning sour gas or landfill gas
  • 4-stroke cycle gas engines in wastewater treatment plants fueled by digester gas
  • 4-stroke cycle converted irrigation engines running on natural gas or LPG
  • Other 4-stroke cycle natural gas engines where the manufacturer specifies a mid-ash gas engine oil
Features/Benefits:
  • Excellent resistance to oxidation and nitration
  • High alkaline reserve to combat acidic combustion by-products when burning sour gas
  • High dispersancy protects against sludge and varnish formation
  • Protects against scuffing and wear
  • Protects against rust and corrosion
  • Excellent low-temperature performance
  • Does not contain any bright stock, which can cause harmful carbon deposits

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/cc
Density 0.877 g/cc0.0317 lb/in³
Viscosity Measurement 111111Index
Kinematic Viscosity at 40°C (104°F) 138 cSt138 cSt
Kinematic Viscosity at 100°C (212°F) 15.1 cSt15.1 cSt
Ash 1.0 %1.0 %Sulfated; ASTM D874
ASTM Color 3.53.5ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Base Number 7.97.9ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -27.0 °C-16.6 °F
Flash Point 260 °C500 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 0.097 %0.097 %
Zinc, Zn 0.109 %0.109 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5354 / 198607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.