MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco 46 Heat Transfer Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nontoxic, noncorrosive, low odor level, excellent seal compatibility fluids that can absorb heat quickly and transport it to the material or fluid requiring heat.

Their excellent thermal and oxidation stability provides long service life and clean heat exchanger systems. There are many uses of heat in processing materials. There are also many ways of transferring heat to the material or fluid that needs to be heated. Chevron Heat Transfer Oils are excellent for this purpose and offer many advantages. They can be used at low pressures. In most applications, the equipment required to apply the oils is relatively inexpensive. The application equipment can also be portable and, therefore, used where it is needed.

Applications

Chevron Heat Transfer Oils are recommended for use in heat transfer systems where fuel oil, gas, or electricity is used to heat a fluid, which then transfers the heat to the point of application.

In closed, forced circulation systems equipped with expansion tanks, Chevron Heat Transfer Oil Grade 22 can be used with bulk oil temperatures up to 316°C (600°F) and skin temperatures up to 343°C (650°F) where good thermal stability and pumpability are required. Chevron Heat Transfer Oil Grade 22 is also ideal where high heat transfer rates combine with high flow rates, and for systems where repeated heating and cooling cycles are required.

In closed or open systems, Chevron Heat Transfer Oil Grade 46 can be used where bulk oil temperatures do not exceed 288°C (550°F) and skin temperatures may be as high as 316°C (600°F). The oil surface in contact with air in open systems should not exceed 107°C (225°F).

Copper and copper alloys should not be used in heat transfer systems with a hydrocarbon fluid unless air (oxygen) is excluded from contact with the fluid by hermetic sealing and/or an inert gas "blanket."

Key Words: CPS Number: 231709; MSDS Number: 4610
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity  0.3215 g/cc
@Temperature 350 °C
0.3215 g/cc
@Temperature 662 °F
 0.668 g/cc
@Temperature 300 °C
0.668 g/cc
@Temperature 572 °F
 0.7032 g/cc
@Temperature 250 °C
0.7032 g/cc
@Temperature 482 °F
 0.7416 g/cc
@Temperature 200 °C
0.7416 g/cc
@Temperature 392 °F
 0.7763 g/cc
@Temperature 150 °C
0.7763 g/cc
@Temperature 302 °F
 0.8105 g/cc
@Temperature 100 °C
0.8105 g/cc
@Temperature 212 °F
 0.8425 g/cc
@Temperature 50.0 °C
0.8425 g/cc
@Temperature 122 °F
 0.8745 g/cc
@Temperature 0.000 °C
0.8745 g/cc
@Temperature 32.0 °F
API Gravity 32 °32 °
Viscosity Measurement 101101Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 212 SUS212 SUS
Saybolt Viscosity at 210°F 47.4 SUS47.4 SUS
Kinematic Viscosity at 40°C (104°F) 41.1 cSt41.1 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 6.32 cSt6.32 cStASTM D445
Vapor Pressure  0.000 bar
@Temperature 0.000 °C
0.000 torr
@Temperature 32.0 °F
 4.00e-8 bar
@Temperature 50.0 °C
0.0000300 torr
@Temperature 122 °F
 2.67e-7 bar
@Temperature 100 °C
0.000200 torr
@Temperature 212 °F
 0.0000227 bar
@Temperature 150 °C
0.0170 torr
@Temperature 302 °F
 0.000467 bar
@Temperature 200 °C
0.350 torr
@Temperature 392 °F
 0.00667 bar
@Temperature 250 °C
5.00 torr
@Temperature 482 °F
 0.0213 bar
@Temperature 300 °C
16.0 torr
@Temperature 572 °F
 0.0533 bar
@Temperature 350 °C
40.0 torr
@Temperature 662 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  1.81 J/g-°C
@Temperature 0.000 °C
0.432 BTU/lb-°F
@Temperature 32.0 °F
 1.99 J/g-°C
@Temperature 50.0 °C
0.476 BTU/lb-°F
@Temperature 122 °F
 2.18 J/g-°C
@Temperature 100 °C
0.520 BTU/lb-°F
@Temperature 212 °F
 2.36 J/g-°C
@Temperature 150 °C
0.563 BTU/lb-°F
@Temperature 302 °F
 2.54 J/g-°C
@Temperature 200 °C
0.607 BTU/lb-°F
@Temperature 392 °F
 2.72 J/g-°C
@Temperature 250 °C
0.650 BTU/lb-°F
@Temperature 482 °F
 2.90 J/g-°C
@Temperature 300 °C
0.694 BTU/lb-°F
@Temperature 572 °F
 3.08 J/g-°C
@Temperature 350 °C
0.737 BTU/lb-°F
@Temperature 662 °F
Thermal Conductivity  0.1096 W/m-K
@Temperature 350 °C
0.7608 BTU-in/hr-ft²-°F
@Temperature 662 °F
 0.1134 W/m-K
@Temperature 300 °C
0.7872 BTU-in/hr-ft²-°F
@Temperature 572 °F
 0.1171 W/m-K
@Temperature 250 °C
0.8124 BTU-in/hr-ft²-°F
@Temperature 482 °F
 0.1207 W/m-K
@Temperature 200 °C
0.8376 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.125 W/m-K
@Temperature 100 °C
0.864 BTU-in/hr-ft²-°F
@Temperature 212 °F
 0.128 W/m-K
@Temperature 150 °C
0.888 BTU-in/hr-ft²-°F
@Temperature 302 °F
 0.1316 W/m-K
@Temperature 50.0 °C
0.9132 BTU-in/hr-ft²-°F
@Temperature 122 °F
 0.1352 W/m-K
@Temperature 0.000 °C
0.9384 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Pour Point -15.0 °C5.00 °FASTM D97
Flammability Test 271271Fire Point °C
 315315Autoignition Point, °C
Flash Point 240 °C464 °FASTM D92
 
Descriptive Properties
Ramsbottom Carbon Residue, wt%0.05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco 22 Heat Transfer Oil
ConocoPhillips Hydroclear® Heat Transfer Oil
ChevronTexaco Rykon® ISO 46 Premium Oil
ChevronTexaco Rando® HD 46
Syensqo (Solvay Specialty Polymers) Galden® HT55 PFPE Heat Transfer Fluid

WCHEV316 / 74931

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.