MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess LEWATIT® MonoPlus S 108 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus S 108 is a strongly acidic, gel-type cation exchange resin in the Na-form with beads of a uniform size (monodisperse) based on a styrene-divinylbenzene copolymer. This resin type is extremely resistant to chemical, osmotic and mechanical stress. That leads to very low leachables even under critical conditions like high temperatures, presence of oxidants (O2, Fe-oxides) and external regeneration processes. Even at very short cycle times (one cycle = service + regeneration) the special ion exchange resin matrix leads to long life cycles in demineralization processes. The high total capacity results in high operating capacities with a very low ionic leakage and a very high regenerant utilization. The extremely high monodispersity [uniformity coefficient: 1.05 (+/- 0.05)] and very low fines content of max 0.1% (<0.4 mm) results in particularly low pressure losses paired with an efficient and cost optimized operation of demineralization plants. Lewatit MonoPlus S 108 is especially suitable for:
  • demineralization of water for industrial steam generation operated with co-current or modern counter-current systems like e.g. Lewatit WS System Lewatit Liftbed System or Lewatit Rinsebed System
  • polishing using the Lewatit Multistep System or a conventional mixed bed arrangement in combination with the following anion components: Lewatit MonoPlus M 500 MB, Lewatit MonoPlus M 800, Lewatit MonoPlus M 600, Lewatit MonoPlus MP 500, Lewatit MonoPlus MP 800 and Lewatit MonoPlus MP 600.
Lewatit MonoPlus S 108 adds special features to the resin bed:
  • high flow rates during regeneration and loading
  • a high operating capacity at low regenerant consumption
  • a low demand for rinse water
  • a homogeneous throughput of regenerants, water and solutions, resulting in a homogeneous operation zone
  • a virtually linear pressure drop gradient across the entire bed depth, allowing operation ith higher bed depths
  • a low TOC emission and high resistance to oxidative stress
  • a good separation of the components in mixed bed applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.840 g/cc0.0303 lb/in³
Density 1.30 g/cc0.0470 lb/in³
Bead Size 0.570 - 0.670 mm0.0224 - 0.0264 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBlack-brown
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8798 / 209190

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.