MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay MIRACARE® 1673 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: High perforance base for the preparation of mild DEA free cleansing products

Chemical Name: SKIN CLEANSER CONCENTRATE

I.N.C.I.. Name: Water (and) Sodium Laureth Sulfate (and) Disodium Laureth Sulfosuccinate (and) Sodium Laureth-6 Carboxylate (and) Ammonium Chloride (and) Cocamidopropyl Betaine

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE® 1673 is a specially formulated skin cleanser base. This concentrate utilizes licensed European technology which takes advantage of the low skin irritation potential of cryptoanionics. These ultra-pure cosmetic quality alkyl polyethoxy carboxylates are supported in their cleansing, foaming and viscosity building characteristics by synergistic combination with selected alkyl polyethoxy sulfosuccinates and sulfates. MIRACARE© 1673 is designed for easy use by simple let-down with water to give a crystal clear, water-white end product useful for facial scrub, skin and body cleansing and/or shampoo. The resulting end products utilizing MIRACARE© 1673 will yield very mild products with low skin and eye irritation.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 34 - 36 %
@Temperature 105 °C,
Time 7200 sec
Sand; RP-0544
pH 5.5 - 6.510% Solution; RP-0420
Viscosity 8300 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear LiquidRP-0064
Color<100APHA, 50% Solution, RP-0134
Foreign MatterFree of Foreign MatterRP-0636

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD230 / 137461

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.