(Viewing data as-entered.
Click here
to return)
Envalior Akulon® K240-HP PA6-I, Conditioned, Heat Stabilized, Impact Modified, Extrusion Blow Molding
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Heat Stabilized
;
Nylon 6, Impact Grade
Material Notes:
Heat Stabilized, Impact Modified, Extrusion Blow Molding
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.10
g/cc
ISO 1183
Mechanical Properties
Original Value
Comments
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
ISO 179/1eU
NB
@Temperature -30.0 °C
ISO 179/1eU
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Hostaform® T 1020 Extrusion Blow Molding Grade Acetal Copolymer
Envalior Akulon® K240-HP PA6-I, Dry, Heat Stabilized, Impact Modified, Extrusion Blow Molding
A. Schulman Diamond DIAMALOY VP22 NATURAL 1001B Blow Molding Grade, Flame Retardant ABS
A. Schulman Diamond ABSPC 9901B ABS/PC Blow Molding Grade, High Impact
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
PDSM8066 / 184767
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.