MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Piccotac™ 1105-E Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Piccotac™ 1105-E Hydrocarbon Resin is a low molecular weight, aliphatic hydrocarbon resin, derived mainly from dienes and other reactive olefin monomers. This pale-colored, neutral resin is characterized by its tack and tack retention, excellent binding properties, high resistance to moisture, UV stability, and good compatibility and solubility. It is used as a binder in hotmelt road markings, hot-melt coatings, waterproofing compositions, and paints and varnishes, and is particularly suitable as tackifier resin in rubber-compounding applications.

Application/Uses:

  • Assembly
  • Building and Construction
  • Contact Adhesives
  • Hot Melt Adhesives
  • Laminating
  • Solventborne Adhesives
  • Wax Modification
Key Attributes:
  • Excellent compatibility with natural rubber and APO
  • High molecular weight increases cohesion

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
Viscosity  450 cP
@Temperature 180 °C
450 cP
@Temperature 356 °F
Melt
 1600 cP
@Temperature 160 °C
1600 cP
@Temperature 320 °F
Melt
 7000 cP
@Temperature 140 °C
7000 cP
@Temperature 284 °F
Melt
Molecular Weight 1200 g/mol1200 g/molMn
 3300 g/mol3300 g/molMw. Mw/Mn ratio = 2.8
 9500 g/mol9500 g/molMz
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 101 °C214 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 4.04.0ASTM D6166

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5514 / 222708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.