MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess LEWATIT® MonoPlus MP 800 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus MP 800 is a strongly basic, macroporous anion exchange resin (type I) with beads of uniform size (monodisperse) based on a styrene-divinylbenzene copolymer, designed for all demineralization applications. The monodisperse beads have chemical and osmotic stability. The extremely high monodispersity (uniformity coefficient: max 1.1) and very low fines content of max. 0.1% ( <0.315 mm) result in particularly low pressure losses compared with standard resins. Due to its special macroporous structure Lewatit MonoPlus MP 800 stands for effective adsorption and desorption of naturally occurring organic substances. Lewatit MonoPlus MP 800 is especially suitable for:
  • polishing using the Lewatit Multistep System or a conventional mixed bed arrangement in combination with Lewatit MonoPlus SP 112 H or Lewatit MonoPlus S 112 H
  • condensate polishing in combination with the Lewatit MonoPlus SP 112 H
  • demineralization of water for industrial steam generation, e.g. Lewatit WS System, Lewatit Liftbed System or Lewatit Rinsebed System
Lewatit MonoPlus MP 800 adds special features to the resin bed:
  • high flow rates during regeneration and loading
  • a good utilization of the total capacity
  • a low demand for rinse water
  • a homogeneous throughput of regenerants, water and solutions, resulting in a homogeneous operating zone
  • a virtually linear pressure drop gradient across the entire bed depth, allowing operation with higher bed depths
  • a good separation of the components in mixed bed applications

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density 1.06 g/cc0.0383 lb/in³
Bead Size 0.570 - 0.670 mm0.0224 - 0.0264 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBeige, opaque
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess LEWATIT® MonoPlus SP 112 H Cation Exchange Resin
Lanxess LEWATIT® MonoPlus S 215 KR Cation Exchange Resin

PLANY8794 / 209186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.