MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Class 1 for outdoor weather-exposed applications. The termination assemblies consist of a skirted insulator, high-dielectric constant (High-K) stress control tube, conformable High-K stress controlling compound and built-in environmental top sealing compound. The insulator is made of a dark gray silicone rubber with excellent tracking resistance and hydrophobic properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 5.86 MPa850 psiSilicone Rubber Insulator; ASTM D412
 10.3 MPa1490 psiHigh-K Stress Control Tube; ASTM D412
100% Modulus  0.896 MPa
@Strain 100 %
130 psi
@Strain 100 %
Silicone Rubber Insulator; ASTM D412
 1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
High-K Stress Control Tube; ASTM D412
300% Modulus  1.24 MPa
@Strain 300 %
180 psi
@Strain 300 %
High-K Stress Control Tube; ASTM D412
 2.76 MPa
@Strain 300 %
400 psi
@Strain 300 %
Silicone Rubber Insulator; ASTM D412
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.6
@Frequency 60.0 Hz
3.6
@Frequency 60.0 Hz
Silicone Rubber Insulator, 1000 V, 50% RH; ASTM D150
 22
@Frequency 60.0 Hz
22
@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
 25
@Frequency 60.0 Hz
25
@Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH, 100 mil; ASTM D150
Dielectric Strength  11.8 kV/mm
@Thickness 1.91 mm
300 kV/in
@Thickness 0.0750 in
Environmental Sealing Compound; ASTM D149
 19.7 kV/mm
@Thickness 1.91 mm
500 kV/in
@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
Dissipation Factor  0.0030
@Frequency 60 Hz
0.0030
@Frequency 60 Hz
Silicone Rubber Insulator, 1000 V, 50% RH; ASTM D150
 0.10
@Frequency 60 Hz
0.10
@Frequency 60 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
 0.90
@Thickness 2.54 mm,
Frequency 60 Hz
0.90
@Thickness 0.100 in,
Frequency 60 Hz
High-K Stress Control Compound, 1000 V, 50% RH; ASTM D150
Track Resistance 18000 sec18000 sec3.5 kV; ASTM 2303
 
Descriptive Properties
AppearanceDark Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35152 / 169899

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.