MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® Epoxy Coat™ 7000 AR
Categories: Polymer; Thermoset; Epoxy

Material Notes: An acid-resistant, room-temperature cured, 100% solids, epoxy coating. Uses: Ideal coating for chemical storage tanks, dike walls, and containment areas where chemical resistance to acids are needed. Features: High build (8-10 mils), Superior resistance to concentrated acids (including 98% sulfuric), Applies with brush or roller, Excellent adhesion to concrete surfaces, Novolac resin.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 3600 cP3600 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 54.4 °C130 °FTemperature Resistance - Wet
 93.3 °C200 °FTemperature Resistance - Dry
 
Processing PropertiesMetricEnglishComments
Processing Temperature 15.6 - 32.2 °C60.0 - 90.0 °FApplication Temperature
Cure Time 1440 min24.0 hour
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Functional cure
 2880 min
@Temperature 24.0 °C
48.0 hour
@Temperature 75.2 °F
Full service
 14400 min
@Temperature 24.0 °C
240 hour
@Temperature 75.2 °F
Full Chemical Cure
Pot Life 36.0 min
@Temperature 23.9 °C
36.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent ResistanceAcetic (Dilute): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 36%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methylene Chloride: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Nitric 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Nitric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Phosphoric 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 40%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayCured
Coverage200 ft²Cured. @ 16 mils
Mix Ratio by volume1.5:1
Mix Ratio by weight1.7:1
Recoat Time4 to 6 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9209 / 239718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.