MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 73G30T BK261 PA6-IGF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Toughened, Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccDAM; ISO 1183
Melt Density 1.19 g/cc
@Temperature 270 °C
Moisture Absorption 2.00 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmDAM; ISO 294-4, 2577
Melt Flow 12.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 105 MPa50% RH; ISO 527-1/-2
 160 MPaDAM; ISO 527-1/-2
Elongation at Break 3.5 %DAM; ISO 527-1/-2
 7.0 %50% RH; ISO 527-1/-2
Tensile Modulus 5600 MPa50% RH; ISO 527-1/-2
 9000 MPaDAM; ISO 527-1/-2
Flexural Modulus 5000 MPaPV; ISO 178
 7800 MPaPV; ISO 178
Poissons Ratio 0.34DAM
 0.3550% RH
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1U
 75.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -30.0 °C
PV,DS; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
PV,DS; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 4.00 µm/m-°CDAM; ISO 11359-1/-2
 6.00 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
 25.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CDAM; ISO 11359-1/-2
 84.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 110 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 221 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 206 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 15.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 22.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °COptimum, Injection
 260 - 280 °CRange, Injection
Mold Temperature 50.0 - 100 °CInjection
 80.0 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6-I,GF30,M1CGR,S14-090
Max. screw tangential speed (m/s)0.2Injection
Odor Class3.5VDA 270
Part Marking Code>PA6-IGF30<ISO 11469
PolymerPA6-I-GF30
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-IGF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K224-HG6U PA6-GF33, Conditioned, 33% Glass Filled, Heat Stabilized
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Conditioned)
Celanese Zytel® 73G30L NC010 PA6-GF30
Celanese Zytel® 73G30HSL BK416 PA6-GF30
DuPont Mobility and Materials Zytel® 7335F NC010 PA6

PDSX5356 / 197996

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.