MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax CA 5075 A Expanded Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Foamed

Material Notes: Hifax CA5075A is an advanced polyolefin selected by our customers for use in various expanded Polypropylene (EPP) foaming applications. This grade features a low melting temperature, a low seal initiation temperature and good optics.

Status: Commercial - Active

Availability: Europe; North America

Application: Foamed Sheet; Packaging Foam, and other Foam applications

Processing Method: Extruded Foam

Attribute: Foamable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccMethod A; ISO 1183-1
Melt Flow 7.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 24.0 MPa50 mm/min; ISO 527-1, -2
Tensile Strength, Yield 19.0 MPa50 mm/min; ISO 527-1, -2
Elongation at Break 450 %50 mm/min; ISO 527-1, -2
Elongation at Yield 14.0 %50 mm/min; ISO 527-1, -2
Flexural Modulus 600 MPa2 mm/min, Chord; ISO 178
Charpy Impact, Notched 7.00 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 115 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9101 / 324036

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.