MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips Synfluid® PAO 8 cSt Polyalphaolefin Lubricant
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Synfluid® PAO 8 cSt can be used in many industrial and automotive lubricant applications. These include gear oils, compressor oils, engine oils, hydraulic fluids, greases, and other functional fluids.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.8326 g/cc
@Temperature 15.6 °C
Density 0.831 g/cc
Volatiles 3.5 %Noack, wt%
Viscosity Measurement 138Viscosity Index
Viscosity Measure 19574 cSt
@Temperature -40.0 °C
Kinematic Viscosity
Kinematic Viscosity at 40°C (104°F) 46.4 cSt
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.030
 
Thermal PropertiesOriginal ValueComments
Pour Point -68.0 °F
Flash Point 504 °F
 
Descriptive Properties
AppearanceClear and bright
Bromine Index<200
Color, Pt-Co0
Fire Point559°F
Odornone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEVP9935 / 242018

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.