Characteristics:- Bimodal molecular weight distribution
- Good tear strength
- Good impact strength
- Good processability
- Excellent bubble stability
Applications: - T-shirt sacks
- Trash can liners
- Merchandise bags
- Coextruded films
Film tested was produced at 0.8 mil with a 4:1 BUR. Information provided by Bayport Polymers LLC. |