MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil LD 103.LS Low Density Polyethylene (LDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LD 103 resins are homopolymer industrial film resins with excellent toughness.  LD 103 resins have a low melt index, which provides good impact strength and melt strength over a range of gauges. 

Availability: Latin America, North America. 

Additive: antiblock: 3000ppm; slip: no; thermal stabilizer: yes. 

Applications:  agricultural film, form fill and seal packaging, medium duty shrink film, blend partner, freezer film, rubber bale wrap, co-extrusion films, liners.  Forms: pellets.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1500 psiASTM D882
Film Tensile Strength at Yield, TD 1500 psiASTM D882
Film Elongation at Break, MD 250 %ASTM D882
Film Elongation at Break, TD 610 %ASTM D882
Puncture Energy 19.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 270 gASTM D1922
Elmendorf Tear Strength TD 90 gASTM D1922
Dart Drop Test 120 gASTM D1709A
Film Tensile Strength at Break, MD 4500 psiASTM D882
Film Tensile Strength at Break, TD 3500 psiASTM D882
1% Secant Modulus, MD 29000 psiASTM D882
1% Secant Modulus, TD 37000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 226 °FPeak; ExxonMobil Method
Vicat Softening Point 196 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 9.2 %ASTM D1003
Gloss 54 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98863 / 238245

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.