Amorphous ethylene-propylene rubber with high ENB (ethylidene norbornene) content and a medium Mooney viscosity. The very low ethylene content ensures excellent low temperature properties. The high ENB content contribute to an ultra fast curing of the compound. This grade is very suitable for automotive sponge applications, dense profiles and wiper blades.Information provided by Lanxess. |