MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Latrobe Knocor™ Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel; Air-Hardening Steel; Hot Work Steel

Material Notes: Koncor hot work tool steel is an air-hardening, 5% chromium tool steel with increase carbon and vanadium for extra resistance to abrasion and wear. The carbon and vanadium contents of Koncor hot work tool steel give it wear properties which are comparable to those of D2 cold work steel and M2 high speed steel. Yet, Koncor exhibits improved toughness compared to D2 and M2 at equivalent harnesses. Koncor exhibits minimal size change during heat treatment and has a wide permissible hardening range of 1850 - 2150°F (1010 - 1177°C). This permits variations in heat treatment for optimization of properties. Austenitizing at the lower end of the range gives maximum toughness and austenitizing at the upper end of the range gives maximum wear resistance.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5858Air Cooled from 982°C, 45 minutes
 61.561.5Air Cooled from 1038°C, 30 minutes
 63.863.8Air Cooled from 1177°C, 10 minutes
Machinability 50 - 55 %50 - 55 %1% Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.1 %1.1 %
Chromium, Cr 5.25 %5.25 %
Iron, Fe 87.55 %87.55 %
Molybdenum, Mo 1.1 %1.1 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 4.0 %4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 593°C

NTIMK094 / 19441

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.