High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colors Applications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where high gloss and low coefficient of friction are required Performance grades of polystyrene are engineered to have specific properties. These products can be custom colored. NOVA Chemicals can accurately match your color needs with its leading edge color technology. Injection Speed: Fast Colored material may differ in some properties. All molded samples were an 1/8 inch thick unless noted. Information provided by NOVA Chemicals. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |