MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polyplastics Laperos® E130G VF2201/BK210P Liquid Crystal Polymer
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Standard for SMT. GF reinforced. High flow.

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ISO 1183
Filler Content 30 %30 %Glass fiber
Water Absorption 0.040 %
@Temperature 23.0 °C,
Time 86400 sec
0.040 %
@Temperature 73.4 °F,
Time 24.0 hour
1 mm thickness; ISO 62
Linear Mold Shrinkage, Flow 0.00060 cm/cm
@Thickness 1.00 mm
0.00060 in/in
@Thickness 0.0394 in
Inj. Pressure 79 Mpa; 80x80x1; Standard
Linear Mold Shrinkage, Transverse 0.0066 cm/cm
@Thickness 1.00 mm
0.0066 in/in
@Thickness 0.0394 in
Inj. Pressure 79 MPa; 80x80x1; Standard
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6565ISO 2039-2
Tensile Strength 170 MPa24700 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Flexural Strain at Break 4.2 %4.2 %ISO 178
Charpy Impact, Notched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+15 ohm-cm6.00e+15 ohm-cmIEC 60093
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
IEC 60250
Dielectric Strength  23.0 kV/mm
@Thickness 3.00 mm
584 kV/in
@Thickness 0.118 in
IEC 60243-1
 44.0 kV/mm
@Thickness 1.00 mm
1120 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
IEC 60250
 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 144 sec144 secASTM D495
Comparative Tracking Index 125 V125 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 270 °C518 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-1,2
Flammability, UL94 V-0V-0
 
Descriptive Properties
Yellow Card File No.E106764

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9935 / 305608

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.