MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel Aquamet® 22 Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: AQUAMET 22 is a high-alloy stainless steel with superior corrosion resistance along with excellent toughness and high strength. It has higher strength than AQUAMET 17 in 3/4" to 1-1/4" dia., and it has equivalent in strength in 1-3/8" to 2" dia. Due to its high alloy content, AQUAMET 22 resists pitting and crevice corrosion and is ideal for pleasure boats which are operated infrequently, spending much of their time tied up at docks. AQUAMET 22 H.S. is a high strength version available in 2-1/2" - 6" dia. NOTE: The mechanical properties of AQUAMET 22 H.S. are slightly lower in sizes 5" dia. and over.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  862 MPa
@Thickness 127 - 152 mm
125000 psi
@Thickness 5.00 - 6.00 in
Aquamet 22 HS
 1000 MPa
@Thickness 19.0 - 31.8 mm
145000 psi
@Thickness 0.750 - 1.25 in
Tensile Strength, Yield  414 MPa
@Strain 0.2 %,
Thickness 127 - 152 mm
60000 psi
@Strain 0.2 %,
Thickness 5.00 - 6.00 in
Tension; Aquamet 22 HS
 621 MPa
@Strain 0.2 %,
Thickness 127 - 152 mm
90000 psi
@Strain 0.2 %,
Thickness 5.00 - 6.00 in
Tension; Aquamet 22 HS
 896 MPa
@Strain 0.2 %,
Thickness 19.0 - 31.8 mm
130000 psi
@Strain 0.2 %,
Thickness 0.750 - 1.25 in
Tension
Elongation at Break 15 %15 %in 2"; 5" to 6"; Aquamet 22 HS
 18 %18 %in 2"; 3/4" to 1-1/4"
Reduction of Area 50 %50 %1-1/4" to 12"
 45 %
@Thickness 19.0 - 31.8 mm
45 %
@Thickness 0.750 - 1.25 in
Shear Strength 597 MPa
@Strain 0.2 %,
Thickness 19.0 - 31.8 mm
86600 psi
@Strain 0.2 %,
Thickness 0.750 - 1.25 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Chromium, Cr 20.5 - 23.5 %20.5 - 23.5 %
Iron, Fe >= 51.87 %>= 51.87 %As Remainder
Manganese, Mn 4.0 - 6.0 %4.0 - 6.0 %
Molybdenum, Mo 1.5 - 3.0 %1.5 - 3.0 %
Nb + Ta 0.10 - 0.30 %0.10 - 0.30 %
Nickel, Ni 11.5 - 13.5 %11.5 - 13.5 %
Nitrogen, N 0.20 - 0.40 %0.20 - 0.40 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Vanadium, V 0.10 - 0.30 %0.10 - 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel Aquamet® 17 Martensitic Steel
Type 431 Martensitic Stainless Steel, Intermediate Temper Forgings, UNS S43100
Outokumpu 2205 Duplex Stainless Steel
Crucible Steel Aquamet® 19 Stainless Steel
Crucible Steel 431 Chromium Steel

NCRUC031 / 16024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.