MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).

Application: For the production of elastic, multi-shock absorbing expanded foams.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.0160 - 0.0350 g/cc
Density 0.0250 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 0.100 MPa
 0.150 MPa
 0.200 MPa
 0.300 MPa
 0.625 MPa
Flexural Strength 0.237 MPa0% E-por Content; DIN 53423
 0.247 MPa60% E-por Content; DIN 53423
 0.257 MPa100% E-por Content; DIN 53423
 0.330 MPaDIN-EN 12089
Compressive Strength 0.115 MPa
@Strain 10 %
DIN-EN 826
 0.145 MPa
@Strain 25 %
DIN-EN 826
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Descriptive Properties
Commercial StatusEurope
Cushioning2.73h/d=15; DIN 55471
Energy Absorption12.5 JHysteresis at 70% compression, v=% mm/min; ISP 3386-1
Flexural Work to Break0.2270% E-por Content; DIN 53423
 0.24760% E-por Content; DIN 53423
 0.25100% E-por Content; DIN 53423
 6.3 JDIN-EN 12098

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
LG Chemical R160 EPS, Flame Retardant
LG Chemical R320 EPS, Flame Retardant
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)

PBASG0083 / 131717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.