MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
PoolKemie SILIMOLD AD-12 RTV2 silicon moulding rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Introduction: It is a two component room temperature vulcanizing pourable fluid silicon which cures on the addition of the appropriate CATALYST AD, according to the polyaddition process. SILIMOLD AD 12 silicon rubber is characterized by its low hardness and a high tearing resistance. Thanks to these properties, it may also be utilized in the manufacture of complex moulds with many undercuts.

Application: SILIMOLD AD 12 silicon rubber is especially designed for complex moulds, model prototype and mould making. Serial realization of polyester, epoxy, polyurethane, cement and wax objects. Pad printing.

Peculiarities: Addition cure; Easy pour able; High tear strength; Extreme mould release/mould life

Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 1:1

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5000 cPComp. A, Before Catalysis, see note 1
 5000 cPComp. B, Before Catalysis, see note 1
Linear Mold Shrinkage 0.0010 cm/cmafter 5 days ageing, After Catalysis; ISO 4823
Storage Temperature 10.0 - 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 10 - 14After Catalysis; DIN 53505
Tensile Strength 2.50 - 3.50 MPaAfter Catalysis; DIN 53504 - S A 3
Elongation at Break 570 - 630 %After Catalysis; DIN 53504 - S A 3
Tear Strength 17.5 - 18.5 kN/mAfter Catalysis; ASTM D 624 S A 3
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hourDemoulding time, See note 1, During Catalysis
Pot Life 25.0 - 35.0 minSee note 1, During Catalysis
Shelf Life 12.0 MonthBoth components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
 
Descriptive Properties
AppearanceFlexible rubberAfter Catalysis
 Thick LiquidBefore Catalysis
ColorOrangeComponent B, Before Catalysis
 OrangeAfter Catalysis
 WhiteComponent A, Before Catalysis
Mixing ratio1:1by weight, Before Catalysis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK014 / 318493

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.