MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Redwood Plastics Redco™ ACRYLIC HiGH IMPACT
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.17 g/cc0.0415 - 0.0423 lb/in³ASTM D792
Water Absorption 0.30 %
@Thickness 3.17 mm,
Time 86400 sec
0.30 %
@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6868ASTM D785
Hardness, Rockwell R 9999ASTM D785
Tensile Strength 37.2 - 48.3 MPa5400 - 7000 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Tensile Modulus 1.52 - 2.21 GPa220 - 320 ksiASTM D638
Flexural Strength 48.3 - 72.4 MPa7000 - 10500 psiASTM D790
Flexural Modulus 1.59 - 2.21 GPa230 - 320 ksiASTM D790
Izod Impact, Notched 0.320 - 0.641 J/cm0.600 - 1.20 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Dielectric Constant  2.5 - 3.0
@Frequency 1e+6 Hz
2.5 - 3.0
@Frequency 1e+6 Hz
ASTM D150
 3.9
@Frequency 1000 Hz
3.9
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.1 - 17.7 kV/mm
@Thickness 3.17 mm
383 - 450 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.010 - 0.020
@Frequency 1000 Hz
0.010 - 0.020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 38.0 µm/m-°C21.1 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 187 °C369 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 - 190 °C338 - 374 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Transmission, Visible 90 %90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW111 / 296677

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.