HX-064AB is a fully-crosslinked thermoplastic elastomer(TPE) product. TPEs can be easily processed with general thermoplastic processing equipment. It has low compression set, good weatherability and excellent resistance to high temperature, chemicals, and ozone. Flexible PVC, rubbers (CR, NBR, EPDM etc.) can be replaced with TPE. Applications: Air Intake Hose, Hose etc. Information provided by Lotte Advanced Materials. |