MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Traid Villarroya TKG® Glass fiber G10 Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy

Material Notes: The most versatile all-around laminate, this grade is made of woven glass fabric impregnated with an epoxy resin binder. It has extremely high mechanical strength, good dielectric loss properties, and good electric strength properties, both in wet and dry conditions.

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³DIN 53 479
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 250 MPa36300 psiDIN 53 455
Modulus of Elasticity 18.0 GPa2610 ksiDIN 53 452
Flexural Strength 400 MPa58000 psiDIN 53 452
Compressive Strength 250 MPa36300 psiDIN 53 454
Tensile Impact Strength 60.0 - 100 kJ/m²28.6 - 47.6 ft-lb/in²Notched, ak10/ak15; DIN 53 453
 130 kJ/m²61.9 ft-lb/in²ak10/ak15; DIN 53 453
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 20.0 µm/m-°C5.56 - 11.1 µin/in-°FVDE 0304
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FDIN 52 672
Maximum Service Temperature, Air 130 °C266 °Flong term
 
Descriptive Properties
Bonding strength4000 NDIN 53 463
Resistance between plugs51000000000[?], DIN 53482
Resistance to tracking200Method KC (DIN 53 480)
Test Voltage II/I55 KVE4, DIN 53 481
 55 KV70, DIN 53 481
Water absorption30 mgE24/50; DIN 53 495

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID951 / 318918

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.