MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen CRP 100 RESIST CR W BLUE High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen CRP 100 RESIST CR W blue is a high density polyethylene (HDPE), dark blue colored similar RAL 5005 with high melt viscosity for extrusion, injection and compression molding. The compound fulfills the material requirements of EN 12201-1 and ISO 4427-1. The product is classified as PE 100-RC and provides a very good long term hydrostatic strength. Especially developed for non-conventional pipe installation methods the product has a superior resistance to slow crack growth. It fulfills the material requirements of PAS 1075:2009-04. Designation acc. ISO 1872-1: PE, EACHL, 50 - T003. Applications: Drinking Water Pipe, Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183-1
Oxidative Induction Time (OIT) 30 minISO 11357-6
Melt Flow 0.27 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 7.3 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63
@Time 3.00 sec
ISO 868
Tensile Strength, Yield 23.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 350 %ISO 527-1,-2
Elongation at Yield 9.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1050 MPaISO 527-1,-2
Flexural Modulus 330 MPacreep, 4 point loading/ 2000 hr; DIN 16841
 560 MPacreep, 4 point loading/ 24 hr; DIN 16841
 1100 MPacreep, 4 point loading/1 min; DIN 16841
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1eA
 26.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
Tensile Creep Modulus, 1 hour 850 MPa
@Pressure 2.00 MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours 360 MPa
@Pressure 2.00 MPa
ISO 899-1
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 74.0 °CB50; ISO 306
DSC Induction Temperature 129 °CDSC
 
Descriptive Properties
FNCT (hrs)>8760ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
MRS Classification (MPA)10ISO 9080
Odor Threshold<=2, EN 1622/EN 1420, measured on pellets/30°C/4 h extraction time
Processing Methodpipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen CRP 100 RESIST S BROWN High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 RESIST S BLUE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 RESIST CR orange High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 ORANGE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Petrothene® LM600731X01 High Density Polyethylene, Sheet Extrusion Grade

PEQT8466 / 220101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.